Inconel 625 Superalloy
Inconel 625 is a nickel-based high temperature deformation alloy, mainly niobium and molybdenum elements as strengthening elements. Inconel 625 superalloy has very good corrosion resistance and is an excellent material in the resistance to crevice corrosion and crack resistance, and has a high degree of resistance in acidic media and organic acids.
1.Characteristics Of Inconel 625 Superalloy
- 1. Strong corrosion resistance, gap corrosion and corrosion between crystals.
- 2. Excellent mechanical properties can be maintained at high and low temperatures.
- 3. Almost completely immune to stress corrosion cracks caused by chlorine gas.
- 4. High temperature to 1050 degrees Celsius, with high antioxidant capacity.
- 5. Good acid resistance, high heat transfer in the construction of thin structure in the environment of acid and alkali medium.
2.Chemical Elements Of Inconel625 Superalloy
Inconel 625 | Ni | Cr | Mo | Al | Ti | Fe | Co |
Element% | 58 | 20-23 | 8-10 | <4.0 | <4.0 | <5.0 | <1.0 |
C | Si | Mn | P | S | Nb | ||
<0.01 | <0.5 | <0.5 | <0.015 | <0.015 | 3.15-4.15 |
3.Applications of Inconel 625 superalloy
1.Aerospace ultra-low temperature, high temperature, good tensile properties and fatigue resistance, widely used in aerospace engine parts. Aerospace structural parts, etc.
2. Marine engineering, seawater parts with high mechanical stress.
3. Oil and gas installations, which exceed 150 degrees Celsius, hydrogen sulfide and other industries.
4. Torch chimneys on offshore oil platforms.
5. Hydrocarbon processing, mainly in the recovery of tar sands and oil shale.

- Tensile strength Rm N/mm2: ≥830
- Yield strength RP0.2N /mm2: ≥410
- Brinell hardness A 5% : 230
- Elongation HB: ≥30
TOP STAR METAL Supply
Titanium and titanium alloy, titanium capillaries, high-precision capillaries, Harloy alloy, superalloy, expansion alloy, nickel-based alloy, Inconel alloy, Incoloy, cobalt-based alloy, copper-nickel alloy, nickel-titanium memory alloy and other materials capillary tube, coil, heat exchanger tube, condenser, plate, bar, forgings, forged rings and other products.