TB6 (Ti10V2Fe3Al) Titanium Alloy Forged Ring

TB6 (Ti10V2Fe3Al) Titanium Alloy

Ti10V2Fe3Al Titanium Alloy

Ti10V2Fe3Al Titanium Alloy Forging Ring

Elastic modulus at room temperature: 104GPa

Phase transition temperature: 800 degrees Celsius

Hardness 335~375HB

Tensile strength: 1200MPa

Product Details

Ti10V2Fe3Al Titanium Alloy is a typical near-β type titanium alloy, containing 3% stable element Al,10% isomorphic β stable element V and 2% eutectoid β stable element Fe. The alloy has strong stress and corrosion resistance, excellent hardenability, good fracture toughness, high specific strength, low forging temperature, low flow stress, and is often used in aerospace parts, landing gear, wings and other parts.

Chemical Element Of Ti10V2Fe3Al Titanium Alloy

Ti10V2Fe3Al Al V Fe C N H Y 0 Ti
Elements 2.6-3.4 9.0-11.0 1.6-2.2 0.05 0.05 0.015 0.005 0.13 Other

Ti10V2Fe3Al Performance

  • Elastic modulus at room temperature: 104GPa
  • Phase transition temperature: 800 degrees Celsius
  • Hardness 335~375HB
  • Tensile strength: 1200MPa

Ti10V2Fe3Al Titanium Alloy Heat Treatment

The alloy adopts isothermal forging, direct water quenching, and aging process, which can shorten the heat treatment period and improve the fracture toughness of the alloy.

Ti10V2Fe3Al Titanium Alloy Processing

TB6 (Ti10V2Fe3Al) Titanium Alloy Forged Ring
TB6 (Ti10V2Fe3Al) Titanium Alloy Forged Ring